Settings according to http://www.nxp.com/documents/mounting_and_soldering/AN10365.pdf - atben.pro, atben.brd, atusb.pro, atusb.brd: set solder mask clearance to 50 um (copper-defined pads) - atben.pro, atben.brd, atusb.pro, atusb.brd: set solder paste clearance to 25 um |
||
---|---|---|
.. | ||
cam | ||
case | ||
sim | ||
tests | ||
atben.brd | ||
atben.cmp | ||
atben.pro | ||
atben.sch | ||
ERRATA | ||
Makefile | ||
MAP | ||
README |
PCB manufacturing: - do not print PCB edges on front/back copper - do not print component values on silk screen - note that the transceiver is "upside down" - the center (!) of the board edge line marks the true board edge, e.g., Edge line (5 mil) ======= ------- - - - - - ---------- | | PCB outside | | PCB inside | | ------- - - - - - ---------- | Volume removed when cutting (width depends on tool used)